Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 992 - 992 g/m²/day @Temperature 38.0 - 38.0 °C |
63.9 - 63.9 g/100 in²/day @Temperature 100 - 100 °F |
Average value: 992 g/m²/day Grade Count:1 |