Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.490 - 6.00 g/m²/day | 0.0316 - 0.386 g/100 in²/day | Average value: 3.08 g/m²/day Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |