Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 4.04 g/m²/day @Temperature 38.0 °C |
0.260 g/100 in²/day @Temperature 100 °F |
90% RH; ExxonMobil Method |
ExxonMobil Bicor™ 21MB866 OPP Film Product Description: Bicor 21MB866 is a high gas barrier, transparent biaxially oriented polypropylene film coated on side acrylic, one side PVOH. It provides excellent gas and aroma protection and .. |