Polymer Property : Water Vapor Transmission = 3.35 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 52.0 g/m²/day

@Temperature 38.0 °C
3.35 g/100 in²/day

@Temperature 100 °F
90% RH; 1 µm
Solvay Specialty Polymers Diofan® P530 Polyvinylidene Chloride (PVDC)  (discontinued **)
DIOFAN® P530 is an one-component latex, water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. Developed..