Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Diofan® P530 Polyvinylidene Chloride (PVDC)  (discontinued **)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® P530 Polyvinylidene Chloride (PVDC)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DIOFAN® P530 is an one-component latex, water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. Developed to adhere on metal and to keep its flexibility with time and in a broad temperature range, it is the ideal binder for one-component, air drying, waterborne formulated paints and coatings where high protection of the substrate is targeted. DIOFAN® P530 combines also high chemical resistance and fire retardant. END USES: - Anticorrosion primers and coatings for industrial and heavy duty steel protection - Automotive primers and underbody coatings - Rust converter products - Barrier and sealing coatings; Flame resistant coatings; Fibers and textile coatings.Additional Information: DELIVERY AND STORAGE: - DIOFAN® P530 will be delivered in bulk or in Intermediate Bulk Containers (IBC). Storage of bulk latex is in reservoirs made of stainless steel, HDPE, rigid PVC or glass fiber reinforced polyester. In particular, metals like iron, zinc, aluminum and copper as well as alloys like brass and bronze have to be avoided for contact with the dispersions. To prevent from drying by evaporation, please keep the vessel tightly closed. To avoid degradation, store the product preferably between 10 and 25°C. REGULATORY INFORMATION - The monomers used for the production of DIOFAN® P530 comply with the requirements of the EU Commission Regulation No. 10/2011 of 14 January 2011. - DIOFAN® P530 complies fully with the U.S. Federal Food, Drug and Cosmetic Act and all applicable food additive regulations. - The monomers used for the production of DIOFAN® P530 comply with the Regulation (EC) 1907/2006 of the European Parliament and of the Council of 18 December 2006 concerning the Registration, Evaluation, Authorization and Restriction of Chemicals (REACH). - SolVin will provide further certification documentation upon request. ISO CERTIFICATION: - The implemented management system for the production, internal transfer and delivery, design and development of DIOFAN vinylidene chloride copolymers (PVDC) produced in Tavaux has been assessed and found to meet the requirements of ISO 9001: 2008, ISO 14001: 2004 and OHSAS 18001: 2007.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
Solids Content 58 %
58 %
pH 1.7
1.7
Water Vapor Transmission 52.0 g/m²/day

@Temperature 38.0 °C
3.35 g/100 in²/day

@Temperature 100 °F
90% RH; 1 µm
Oxygen Transmission Rate 230 cc/m²/day
14.8 cc/100 in²/day
25°C, 1.0 µm, 0% RH
Surface Tension 40 dynes/cm
40 dynes/cm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 13.0 °C
55.4 °F
Film; DSC
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH)
EU No 10/2011
Appearance Milky white liquid
White
Availability Asia Pacific
Europe
North America
Emulsion Type Anionic
Features Barrier Resin
Flame Retardant
Good Adhesion
Good Chemical Resistance
Non-Toxic
Filmability 9°C
Minimum Film Forming Temperature
Forms Liquid
Generic PVDC
Uses Coating Applications
Users viewing this material also viewed the following: