Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | <= 2.00 g/m²/day | <= 0.129 g/100 in²/day | 23°C; 50% RH; ASTM F1249 |
OCTAL DPET™/PE Laminate Sheet with Improved Barrier Properties Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals. |
|||
Water Vapor Transmission | <= 2.00 g/m²/day | <= 0.129 g/100 in²/day | 23°C; 50% RH; ASTM F1249 |
OCTAL DPET™/PE Lock-Up Laminate Sheet Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals. |
|||
Water Vapor Transmission | <= 2.00 g/m²/day | <= 0.129 g/100 in²/day | 23°C; 50% RH; ASTM F1249 |
OCTAL DPET™/PE Peelable Laminate Sheet Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals. |
|||
Water Vapor Transmission | 2.00 g/m²/day | 0.129 g/100 in²/day | ASTM F1249 |
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films.. |