Polymer Property : Water Vapor Transmission = 0.129 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission <= 2.00 g/m²/day
<= 0.129 g/100 in²/day
23°C; 50% RH; ASTM F1249
OCTAL DPET™/PE Laminate Sheet with Improved Barrier Properties
Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals.
Water Vapor Transmission <= 2.00 g/m²/day
<= 0.129 g/100 in²/day
23°C; 50% RH; ASTM F1249
OCTAL DPET™/PE Lock-Up Laminate Sheet
Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals.
Water Vapor Transmission <= 2.00 g/m²/day
<= 0.129 g/100 in²/day
23°C; 50% RH; ASTM F1249
OCTAL DPET™/PE Peelable Laminate Sheet
Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals.
Water Vapor Transmission 2.00 g/m²/day
0.129 g/100 in²/day
ASTM F1249
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer
Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films..