Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 4.05 g/m²/day | 0.261 g/100 in²/day | ASTM D1653 |
3M Scotchkote™ 206N XTRA LG Fusion Bonded Epoxy Coating Scotchkote Fusion Bonded Epoxy coating 206N XTRA LG is one-part, heat curable, thermosetting, powdered epoxy coating with extended gel for coating the interior of line pipe and fittings, valves, and.. |