Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 2.64 g/m²/day | 0.170 g/100 in²/day | ASTM F1249 |
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Water Vapor Transmission | 2.64 g/m²/day | 0.170 g/100 in²/day | 100°F / 100%RH); ASTM F1249 |
Honeywell Capran® Emblem™ 1200MT Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1200MT is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hy.. |