Neck In 8.13 cm

@Temperature 240 °C
3.20 in

@Temperature 464 °F
328 ft/min, constant output at 35 rpm; ExxonMobil Method
ExxonMobil Escorene™ FL 00714 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00714 is an easy processable grade for extrusion coating, co-extrusion coating and cast film. This grade offers excellent heat sealing characteristics and excellent optical p..