Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 8.13 cm @Temperature 240 °C |
3.20 in @Temperature 464 °F |
328 ft/min, constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escorene™ FL 00714 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00714 is an easy processable grade for extrusion coating, co-extrusion coating and cast film. This grade offers excellent heat sealing characteristics and excellent optical p.. |