Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 10.9 cm @Temperature 230 °C |
4.30 in @Temperature 446 °F |
328 ft/min, constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 726.07 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. LD 716.07 is an excelle.. |
|||
Neck In | 10.9 cm @Temperature 280 °C |
4.30 in @Temperature 536 °F |
328 ft/min, constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escor™ 5100 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5100 is primarily intended for extrusion coating, coextrusion coating and extrusion lamination. Excellent adhesion to polar substrates, aluminum foil, metalized films, pap.. |