Physical Properties Metric English Comments
Neck In 4.57 cm

@Temperature 315 °C
1.80 in

@Temperature 599 °F
328 ft/min, Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LDPE LD 259 Low Density Polyethylene Resin (European Grade)
Product Description: LD 259 is a LDPE extrusion coating grade, especially introduced for coating on non-woven substrates. Its high melt-index combines with low density gives this grade the right bal..