Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 4.32 cm @Temperature 315 °C |
1.70 in @Temperature 599 °F |
328 ft/min, Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil LDPE LD 252 Low Density Polyethylene Resin (European Grade) Product Description: LD 525 is a high purity LDPE extrusion coating grade, designed to meet environmental needs for reduced fume emissions during plastics conversion. This grade offers:Low volatiles.. |
|||
Neck In | 4.32 cm @Temperature 315 °C |
1.70 in @Temperature 599 °F |
656 ft/min, Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil LDPE LD 258 Low Density Polyethylene Resin (European Grade) Product Description: LD 258 is a LDPE extrusion coating grade, having superior organoleptic properties compared to existing standard low odor/off-taste LDPE extrusion coating polymers. The developme.. |
|||
Neck In | 4.32 cm @Temperature 315 °C |
1.70 in @Temperature 599 °F |
656 ft/min, Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil LDPE LD 259 Low Density Polyethylene Resin (European Grade) Product Description: LD 259 is a LDPE extrusion coating grade, especially introduced for coating on non-woven substrates. Its high melt-index combines with low density gives this grade the right bal.. |