Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.910 bar @Temperature 25.0 °C |
683 torr @Temperature 77.0 °F |
|
Solvay Specialty Polymers Meforex® 123 Ozone-Friendly CFC Replacement Formula: CHCl2CF3; Name: 1,1 Dichloro 2,2,2 Trifluoroethane. Replaces CFC 11. Industrial air-conditioning, heat pumps, and heat transfer fluid.Information provided by Solvay Solexis, Inc. |