Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Meforex® 123 Ozone-Friendly CFC Replacement

Category Fluid
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name Meforex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Meforex® 123 Ozone-Friendly CFC Replacement.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formula: CHCl2CF3; Name: 1,1 Dichloro 2,2,2 Trifluoroethane. Replaces CFC 11. Industrial air-conditioning, heat pumps, and heat transfer fluid.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.46 g/cc

@Temperature 25.0 °C
0.0527 lb/in³

@Temperature 77.0 °F
Liquid
Molecular Weight 152.9 g/mol
152.9 g/mol
Vapor Pressure 0.910 bar

@Temperature 25.0 °C
683 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Heat of Vaporization 170 J/g
73.1 BTU/lb
at Boiling Point
Melting Point -107.1 °C
-160.8 °F
at 1.013 bar
Boiling Point 27.8 °C
82.0 °F
at 1.013 bar
Chemical Properties Metric English Comments
Critical Pressure 36.68 bar
27510 torr
Critical Temperature 183.8 °C
362.8 °F
Critical Density 0.550 g/cc
0.0199 lb/in³
Descriptive Properties Value Comments
Flammability Range (vol%) None
Ozone Depletion Potential 0.022
Based on CFC11 = 1.0
Toxicity Level 1000 ppm
Allowed limit in work places, values suggested by AIHA (American Industrial Hygiene Association).
Users viewing this material also viewed the following: