Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 2.00e-15 bar | 1.50e-12 torr | |
M Chemical GUARD DOG™ UV1577 Light Absorber, Triazene Derivative GUARD DOG™ UV1577 UV absorber is a low volatile Triazine based UV absorber which is highly effective in polymers that are processed at high temperature (decomposition temperature > 350°C).Ap.. |
|||
Vapor Pressure | 2.00e-15 bar | 1.50e-12 torr | |
M Chemical GUARD DOG™ UV234 Light Absorber, Benzotriazole Derivative GUARD DOG™ UV234 UV absorber is a low volatile benzotriazole based UV absorber which is highly effective in polymers that are processed at high temperature (decomposition temperature > 350°C.. |