Polymer Property : Vapor Pressure = 0.0400 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.0400 bar

@Temperature 20.0 °C
30.0 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil Exxsol™ DSP100/120 Dearomatized Fluid
Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Vapor Pressure 0.0400 bar

@Temperature 20.0 °C
30.0 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil IPA Isopropyl Alcohol
Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil
Vapor Pressure 0.0400 bar

@Temperature 20.0 °C
30.0 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil Isopar™ C Isoparaffin Fluid
Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Asia ..
Vapor Pressure <= 0.0400 bar
<= 30.0 torr
Abatron Acrylic 57-1™ Clear, Water-Based Coating
Acrylic 57-1™ is a high-gloss, non-yellowing acrylic coating. It forms a very clear film with exceptional mar resistance. Because it will not yellow and is stain resistant, it is an excellent choic..
Vapor Pressure 0.0400 bar

@Temperature 50.0 °C
30.0 torr

@Temperature 122 °F
BASF Hexamethylenediamine 70%
Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF