Material Notes:
Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Asia Pacific, Europe, Central America, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.699 g/cc

@Temperature 15.6 °C
0.0252 lb/in³

@Temperature 60.0 °F
ASTM D4052
Kinematic Viscosity 0.72 cSt
0.72 cSt
ASTM D445
Vapor Pressure 0.0400 bar

@Temperature 20.0 °C
30.0 torr

@Temperature 68.0 °F
ExxonMobil Method
Thermal Properties Metric English Comments
Boiling Point 97.8 °C
208 °F
Initial; ASTM D86
Flash Point <= 0.000 °C
<= 32.0 °F
ASTM D56
Descriptive Properties Value Comments
Aniline Point 172°F
Method E, ASTM D611
Aromatic Content 10 wt ppm
ExxonMobil Method
Dry Point 219°F
ASTM D86