Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.0000930 bar | 0.0698 torr | |
3M Novec™ FC-4430 Fluorosurfactant 3M™ Novec™ Fluorosurfactant FC-4430 is a non-ionic polymeric fluorochemical surfactant belonging to a class of coating additives which provide low surface tensions in coating systems best served b.. |
|||
Vapor Pressure | 0.0000930 bar | 0.0698 torr | |
3M Novec™ FC-4432 Fluorosurfactant 3M fluorosurfactant FC-4432 is a non-ionic polymeric fluorochemical surfactant that offers excellent wetting, leveling and flow control in a variety of waterborne, solvent-borne and high-solids orga.. |