Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 965 microns | 38.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 965 - 1070 microns | 38.0 - 42.0 mil | Overall |
Arlon 51586R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mate.. |
|||
Thickness | 965 - 1070 microns | 38.0 - 42.0 mil | Overall |
Arlon 940-10Rxx-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |