Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 203 - 229 microns | 8.00 - 9.00 mil | Side 1 |
Arlon 51576S020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 178 - 229 microns | 7.00 - 9.00 mil | Overall |
Arlon R34172W008 0.008" (0.203 mm) Cured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Cured, Unsupported Silicone Rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 178 - 229 microns | 7.00 - 9.00 mil | Side 1 |
Arlon R34172W008 0.008" (0.203 mm) Cured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Cured, Unsupported Silicone Rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 203 - 229 microns | 8.00 - 9.00 mil | Side 2 |
Arlon R35066R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |