Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 210 microns | 8.27 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51073R031 0.0311" (0.79 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber This data represents typical values for the production materi.. |