Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 51073R031 0.0311" (0.79 mm) Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 51073R031 0.0311" (0.79 mm) Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 74.9 microns
2.95 mil
Interleave
210 microns
8.27 mil
Substrate; Arlon SQA-TMS-003
290 microns
11.4 mil
Side 1; Arlon SQA-TMS-003
290 microns
11.4 mil
Side 2; Arlon SQA-TMS-003
790 microns
31.1 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
Silicone Property; ASTM D2240
81
81
Product Property; ASTM D2240
Tensile Strength 7.79 MPa
1130 psi
Silicone Property; ASTM D412
Elongation at Break 854 %
854 %
Silicone Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 23.0 °C
60.0 Month

@Temperature 73.4 °F
From date of manufacture
Descriptive Properties Value Comments
Color Naturally White
Substrate
Red
Total Product Weight (g/m2) 891
Arlon SQA-TMS-025