Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 188 microns | 7.40 mil | PET |
Aldrich Single Layer Graphene on PET PET film base with graphene coating; uniform film and excellent thickness consistency. Its transparency combined with electrical conductivity allows it use in many niche applications. |
|||
Thickness | 188 microns | 7.40 mil | |
Hexcel® HexForce™ 4533 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 188 microns | 7.40 mil | |
Hexcel® HexForce™ 4797 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 188 microns | 7.40 mil | Typical; ASTM D374 |
DuPont™ Nomex® 414 Paper, 7 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Thickness | 188 microns | 7.40 mil | Substrate |
Arlon 28751R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o.. |