Physical Properties Metric English Comments
Thickness 188 microns
7.40 mil
PET
Aldrich Single Layer Graphene on PET
PET film base with graphene coating; uniform film and excellent thickness consistency. Its transparency combined with electrical conductivity allows it use in many niche applications.
Thickness 188 microns
7.40 mil
Hexcel® HexForce™ 4533 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 188 microns
7.40 mil
Hexcel® HexForce™ 4797 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 188 microns
7.40 mil
Typical; ASTM D374
DuPont™ Nomex® 414 Paper, 7 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..
Thickness 188 microns
7.40 mil
Substrate
Arlon 28751R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o..