Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 180 microns | 7.10 mil | |
Hexcel® HexForce™ 1035 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 180 microns | 7.10 mil | Total |
3M 470 Electroplating Tape 3M™ Electroplating Tape 470 is a conformable and abrasion-resistant vinyl tape with excellent resistance to most chemicals used in typical electroplating processes.Information provided by 3M |
|||
Thickness | 180 microns | 7.10 mil | Total |
3M 470L Electroplating Tape 3M™ Electroplating Tape 470L is a linered version of 3M vinyl tape 470 that may be used for die-cutting or large area applications.Information provided by 3M |