3M 470 Electroplating Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 470 Electroplating Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Electroplating Tape 470 is a conformable and abrasion-resistant vinyl tape with excellent resistance to most chemicals used in typical electroplating processes.Information provided by 3M
Physical Properties Metric English Comments
Thickness 155 microns
6.10 mil
Liner
160 microns
6.30 mil
Backing
180 microns
7.10 mil
Total
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.4 MPa
2810 psi
ASTM D3759
Elongation at Break 180 %
180 %
ASTM D3759
Peel Strength 0.40538 kN/m
2.3125 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Tan