Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 640 microns | 25.2 mil | Standard |
GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the .. |
|||
Thickness | 640 microns | 25.2 mil | Standard |
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall.. |
|||
Thickness | 640 microns | 25.2 mil | Standard |
GrafTech GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC c.. |