Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 163 microns | 6.40 mil | ASTM D3652 |
3M Scotch® 865 Reinforced Strapping Tape Scotch® Strapping Tape is reinforced with continuous polypropylene monofilaments. The polypropylene backing provides excellent abrasion, moisture and scuff resistance. The adhesive is specifically .. |