Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 163 microns | 6.40 mil | ASTM D3652 |
3M Scotch® 865 Reinforced Strapping Tape Scotch® Strapping Tape is reinforced with continuous polypropylene monofilaments. The polypropylene backing provides excellent abrasion, moisture and scuff resistance. The adhesive is specifically .. |
|||
Thickness | 163 - 187 microns | 6.42 - 7.36 mil | |
CEN® Electronic Material CN Polyimide Film, 7 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Thickness | 163 - 187 microns | 6.42 - 7.36 mil | ASTM D374 |
CEN® Electronic Material CV Polyimide Film, 7 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |