Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 14000 microns | 550 mil | ASTM D418-68 |
3M Nomadâ„¢ 8150 Scraper Matting The product is a backed, non-woven, floor matting made from continuous vinyl filaments bonded together. The matting is motor oil resistant and suitable for heavy duty foot traffic in dry or wet area.. |