3M Nomad™ 8150 Scraper Matting

Category Other Engineering Material
Manufacturer 3M
Trade Name Nomad™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Nomad™ 8150 Scraper Matting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The product is a backed, non-woven, floor matting made from continuous vinyl filaments bonded together. The matting is motor oil resistant and suitable for heavy duty foot traffic in dry or wet areas. It also serves to scrape off the collect dirt which helps prevent dirt from being tracked into a building and holds dirt away from the floor surface below.Information provided by 3M
Physical Properties Metric English Comments
Thickness 14000 microns
550 mil
ASTM D418-68
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Minimum Service Temperature, Air 23.0 °C
73.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 7.20e+11 ohm-cm
7.20e+11 ohm-cm
ASTM D257