Physical Properties Metric English Comments
Thickness 102000 - 202000 microns
4020 - 7950 mil
intermediate sizes also available
Superior Die Set FORTAL® HP Aluminum Alloy
Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and d..