Physical Properties Metric English Comments
Thickness 115 microns
4.54 mil
wet film
Aremco Ceramabind™ 542 High Temperature Inorganic Binder
Single part, low viscosity, water-dispersed, aluminum phosphate solution for penetrating ultra fine thermal spray applications to 3000°F (1650°C).