Physical Properties Metric English Comments
Thickness 324 - 396 microns
12.8 - 15.6 mil
Blank on PET
CeramTec Ceramtape GC Glass Ceramic
LTCC (Low Temperature Cofired Ceramic) is a new type of ceramic film developed by CeramTec AG's Electronics division. With the aid of these ceramics and their almost shrinkage-free sintering process..