Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 3940 - 10800 microns | 155 - 425 mil | Range of Thicknesses Available |
Rogers Corporation Poron® 4790-92-12 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |