Polymer Property : Thickness = 10800 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 3940 - 10800 microns
155 - 425 mil
Range of Thicknesses Available
Rogers Corporation Poron® 4790-92-12 Urethane Foam, Extra Soft, Slow Rebound
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..