Physical Properties Metric English Comments
Thickness 914 - 1120 microns
36.0 - 44.0 mil
Overall
Arlon 10502R030 0.040" (1.02 mm) Cured/Post-Cured Unsupported Silicone Rubber
Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used t..
Thickness 914 microns
36.0 mil
Side 2; Arlon SQA-TMS-003
Arlon 51146R050 0.050" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values for the production materi..
Thickness 914 microns
36.0 mil
Overall; Arlon SQA-TMS-003
Arlon 55148R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data r..
Thickness 914 microns
36.0 mil
Overall; Arlon SQA-TMS-003
Arlon 55578R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Appearance:..
Thickness 914 microns
36.0 mil
Overall; Arlon SQA-TMS-003
Arlon R39091R036 0.036" (0.914 mm) Uncured Silicone Rubber with Nomex Fabric Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1574 Nomex FabricSide 2: Uncured SiliconeInterleave: Polyethylene This data represents typical values fo..
Thickness 914 microns
36.0 mil
3M Safety-Walk™ 510 Black Slip-Resistant Conformable Tapes and Treads
A high-friction, slip-resistant material that has a special pressure-sensitive adhesive backed aluminum film that conforms around corners and adheres to irregular surfaces.For irregular or contoured..
Thickness 914 microns
36.0 mil
3M Safety-Walk™ 530 Safety Yellow Slip-Resistant Conformable Tapes and Treads
A high-friction, slip-resistant material that has a special pressure-sensitive adhesive backed aluminum film that conforms around corners and adheres to irregular surfaces.For irregular or contoured..
Thickness 914 microns
36.0 mil
3M Safety-Walk™ 620-B Clear Slip-Resistant General Purpose Tapes and Treads
A mineral-coated, slip-resistant material adhered by a durable resin to a pressure-sensitive adhesive backed plastic film.For light to heavy shoe-traffic areasMineral-coated, high friction slip-resi..
Thickness 914 microns
36.0 mil
3M Safety-Walk™ 630 Safety Yellow Slip-Resistant General Purpose Tapes and Treads
A mineral-coated, slip-resistant material adhered by a durable resin to a pressure-sensitive adhesive backed plastic film.For light to heavy shoe-traffic areasMineral-coated, high friction slip-resi..
Thickness 914 microns
36.0 mil
Adhesive
3M 4411B Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Thickness 914 microns
36.0 mil
Adhesive
3M 4411G Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Thickness 914 microns
36.0 mil
Adhesive
3M 4411N Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..