Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 318 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 318 microns
12.5 mil
Hexcel® HexForce™ GA090 Carbon Fabric
Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper..
Thickness 318 microns
12.5 mil
Hexcel® HexForce™ 7562 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 318 microns
12.5 mil
Side 2; Arlon SQA-TMS-003
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical ..
Thickness 318 microns
12.5 mil
Side 1; Arlon SQA-TMS-003
Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassAppearance: Red silicone rubber on fiberglass fabric.This data represents typical values for the product..
Thickness 318 microns
12.5 mil
Side 1; Arlon SQA-TMS-003
Arlon P29514R020P 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassThis data represents typical values for the production material. The data should..
Thickness 318 - 394 microns
12.5 - 15.5 mil
Overall
Arlon R32021R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
Thickness 318 - 394 microns
12.5 - 15.5 mil
Overall
Arlon R32031R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
Thickness 318 - 394 microns
12.5 - 15.5 mil
Overall
Arlon 51943C014 0.014" (0.356 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, ..
Copyright © lookpolymers.com All Rights Reserved