Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 318 microns | 12.5 mil | |
Hexcel® HexForce™ GA090 Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |
|||
Thickness | 318 microns | 12.5 mil | |
Hexcel® HexForce™ 7562 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 318 microns | 12.5 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 318 microns | 12.5 mil | Side 1; Arlon SQA-TMS-003 |
Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassAppearance: Red silicone rubber on fiberglass fabric.This data represents typical values for the product.. |
|||
Thickness | 318 microns | 12.5 mil | Side 1; Arlon SQA-TMS-003 |
Arlon P29514R020P 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassThis data represents typical values for the production material. The data should.. |
|||
Thickness | 318 - 394 microns | 12.5 - 15.5 mil | Overall |
Arlon R32021R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 318 - 394 microns | 12.5 - 15.5 mil | Overall |
Arlon R32031R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 318 - 394 microns | 12.5 - 15.5 mil | Overall |
Arlon 51943C014 0.014" (0.356 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |