Polymer Property : Thickness = 3100 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 3100 microns
122 mil
Standard; Laminate
GrafTech GRAFOIL® GHR Standard Fluid Sealing Laminate, Metal Reinforced
GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface iden..
Thickness 3100 microns
122 mil
Standard
GrafTech GRAFOIL® GHW Standard Fluid Sealing Laminate, Non-Metal Reinforced
GRAFOIL® Grade GHW is a laminate made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0025" thick high-temperature continuous woven glass fiber insert. Its functional tempera..