Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 3100 microns | 122 mil | Standard; Laminate |
GrafTech GRAFOIL® GHR Standard Fluid Sealing Laminate, Metal Reinforced GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface iden.. |
|||
Thickness | 3100 microns | 122 mil | Standard |
GrafTech GRAFOIL® GHW Standard Fluid Sealing Laminate, Non-Metal Reinforced GRAFOIL® Grade GHW is a laminate made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0025" thick high-temperature continuous woven glass fiber insert. Its functional tempera.. |