Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 800 microns | 31.5 mil | Thickness tested |
Thermoseal RG-N100 PTG Gasketing Thermoseal RG-N100 is a nitrile butadiene rubber, reinforced cellulose fiber and mineral filler general purpose gasket material. Continuous roll lengths allow efficient and economical fabrication wi.. |
|||
Thickness | 800 microns | 31.5 mil | Thickness tested |
Thermoseal RG-N120 PTG Gasketing Thermoseal RG-N120 is a reinforced cellulose gasket material with a nitrile butadiene rubber binder and inorganic fillers that provides a very good crush resistance at high flange pressures. Continu.. |
|||
Thickness | 800 microns | 31.5 mil | Thickness tested |
Thermoseal RG-P160 PTG Gasketing Thermoseal RG-P160 is a blended fiber and polychloroprene rubber gasket material with mineral fillers. A factory applied release coating on both sides aid in flange removal. Continuous roll lengths .. |
|||
Thickness | 800 microns | 31.5 mil | Thickness tested |
Thermoseal RG-S140 PTG Gasketing Thermoseal RG-S140 is a controlled-swell gasket material that provides excellent sealing w here initial gasket conformability is required to compensate for flange out of flatness or roughness. After.. |
|||
Thickness | 800 microns | 31.5 mil | Thickness tested |
Thermoseal RG-S160 PTG Gasketing Thermoseal RG-S160 offers exceptional sealability and crush resistance in a wide range of applications. RG-S160 is composed of a blend of aramid, mineral, and cellulose fibers and graphite and other.. |
|||
Thickness | 800 microns | 31.5 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55579R031H 0.0315" (0.800 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPELayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. T.. |
|||
Thickness | 800 - 1590 microns | 31.5 - 62.5 mil | Average value: 1330 microns Grade Count:3 |
Overview of materials for Chlorosulfonated Polyethylene Rubber This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val.. |