Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 91.4 - 102 microns | 3.60 - 4.00 mil | Range of Thicknesses available |
Rogers Corporation RO4450B Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
Thickness | 91.4 microns | 3.60 mil | |
Hexcel® HexForce™ 1125 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 91.4 microns | 3.60 mil | |
ExxonMobil Label-Lyte® 90 LP Coated, High Sheen, Metallized, White Opaque OPP for Water-based Patch Label Applications Coated, white, metallized polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement. This film is compatible with offset litho and UV-cured in.. |
|||
Thickness | 91.4 microns | 3.60 mil | |
ExxonMobil Label-Lyte® 95 LP Coated, White Opaque OPP for Water-based Patch Label Applications White, polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement on glass, metal, HDPE, and PET containers. It is designed to be used as a mon.. |
|||
Thickness | 91.4 microns | 3.60 mil | Total; ASTM D3652 |
3M 33803 General Purpose Aluminum Foil Tape High tack rubber adhesive. 40 lb liner. UL 723 ClassifiedInformation provided by 3M |
|||
Thickness | 91.4 microns | 3.60 mil | Total; ASTM D3652 |
3M 433 Premium Performance Aluminum Foil Tape Silicone adhesive for high temperature resistance; MIL-T-47014, FAR 25.853, UL 746C Recognized; smooth easy unwind; clean, straight edges with minimal wrinkling.Information provided by 3M |
|||
Thickness | 91.4 microns | 3.60 mil | Liner |
3M FA03J Matte Clear Acetate Label Products 3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate.. |
|||
Thickness | 91.4 microns | 3.60 mil | Liner |
3M FM0196J MC Polyester Label Products 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Thickness | 91.4 microns | 3.60 mil | Liner |
3M FM118J Indoor UL Recognized MC Polyester Label Products 3M™ Indoor UL Recognized MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These po.. |
|||
Thickness | 91.4 microns | 3.60 mil | Liner |
3M FM16J Indoor UL Recognized Computer Imprintable White Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Thickness | 91.4 microns | 3.60 mil | Liner |
3M FM28J Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Thickness | 91.4 microns | 3.60 mil | Total; ASTM D3652 |
3M 3302 Specialty Foil Tape Aluminum foil tape. EMI/RFI shielding. Ul 510 Recognized.Information provided by 3M |
|||
Thickness | 91.4 microns | 3.60 mil | Total; ASTM D3652 |
3M 3311 General Purpose Aluminum Foil Tape Ul 723 listedInformation provided by 3M |
|||
Thickness | 91.4 microns | 3.60 mil | Adhesive |
3M 9453LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 91.4 microns | 3.60 mil | Liner |
3M FM0196J MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Thickness | 91.4 microns | 3.60 mil | Liner |
3M FM14J Indoor UL Recognized Computer Imprintable Clear Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Thickness | 91.4 microns | 3.60 mil | ASTM D3652 |
3M Scotch® 3311 Foil Tape Scotch® Foil Tape 3311 is an aluminum alloy foil with a pressure-sensitive adhesive and paper liner. The aggressive rubber adhesive sticks well to most surfaces and the paper liner makes for conven.. |