Polymer Property : Thickness = 3.48 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 3.48 microns
0.137 mil
ASTM D3652
3M Scotch® 4735 High Temperature Fine Line Tape
Scotch® High Temperature Fine Line Tape 4735 is a vinyl fine line paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are r..
Thickness 3.48 microns
0.137 mil
ASTM D3652
3M Scotch® 4737S High Temperature Fine Line Tape
Scotch® High Temperature Fine Line Tape 4737 is a vinyl paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are required.In..
Thickness 3.48 microns
0.137 mil
ASTM D3652
3M Scotch® 4737T High Temperature Fine Line Tape
Scotch® High Temperature Fine Line Tape 4737 is a vinyl paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are required.In..