3M Scotch® 4735 High Temperature Fine Line Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 4735 High Temperature Fine Line Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® High Temperature Fine Line Tape 4735 is a vinyl fine line paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are required.Information provided by 3M
Physical Properties Metric English Comments
Thickness 3.48 microns
0.137 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.9 MPa
2590 psi
ASTM D3759
Elongation at Break 130 %
130 %
ASTM D3759
Peel Strength 0.10408 kN/m
0.59375 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
for up to 30 mins
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Orange (Translucent)