Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 82.5 microns | 3.25 mil | |
Chengdu Polyster 10 LPI Lenticular Lens Sheet, PS 10 LPI lenticular lens sheet has wider viewing range. It is of high impact resistance and UV resistance. It has been specially designed for outdoor billboards, signboards and shop displays. The sui.. |
|||
Thickness | 82.5 microns | 3.25 mil | |
Chengdu Polyster 20 LPI Lenticular Lens Sheet, PS The image printed by this sheet material is being separated into layers clearly. It has the 3D effect, and has high UV resistance. It has been designed for posters, outdoor billboards, signboards, .. |
|||
Thickness | 82.5 microns | 3.25 mil | Total; ASTM D3652 |
3M 3380 General Purpose Aluminum Foil Tape 40 lb natural kraft paper liner. Good for narrow slit rolls. UL 723 ClassifiedInformation provided by 3M |
|||
Thickness | 82.5 microns | 3.25 mil | Total; ASTM D3652 |
3M 3380 HVAC Construction General purpose aluminum foil tape. Go to product for this market. UL 723 Classified.Information provided by 3M |
|||
Thickness | 82.5 microns | 3.25 mil | Total; ASTM D3652 |
3M 4380 General Purpose Aluminum Foil Tape 3M™ Aluminum Foil Tape 4380 is a general purpose aluminum foil tape offering a dead soft aluminum foil backing combined with an acrylic pressure sensitive adhesive.Information provided by 3M |
|||
Thickness | 82.5 microns | 3.25 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 406 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Thickness | 82.5 microns | 3.25 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 407 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Thickness | 82.5 microns | 3.25 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 413 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Thickness | 82.5 microns | 3.25 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 414 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Thickness | 82.5 microns | 3.25 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 404 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Thickness | 82.5 microns | 3.25 mil | Total; ASTM D3652 |
3M 97065 General Purpose Aluminum Foil Tape 60 lb. moisture stable liner. Good for die-cut applications.Information provided by 3M |
|||
Thickness | 82.5 microns | 3.25 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 405 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |