Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchcal™ ElectroCut™ 414 Graphic Film

Category Polymer , Film
Manufacturer 3M
Trade Name Scotchcal™ ElectroCut™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcal™ ElectroCut™ 414 Graphic Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high attention value under poor visibility, particularly at dawn or duskGood electronic cutting characteristics as small as 12 mm tallPrintable with solvent-based screen print inksGood weather resistanceInformation provided by 3M
Physical Properties Metric English Comments
Thickness 82.5 microns
3.25 mil
without adhesive
102 microns
4.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 8.62 MPa
>= 1250 psi
Peel Strength 0.701 kN/m
4.00 pli
Adhesion to Acrylic
0.701 kN/m
4.00 pli
Adhesion to Glass
0.701 kN/m
4.00 pli
Adhesion to Polycarbonate
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 107 °C
225 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Appearance Red Orange
Users viewing this material also viewed the following: