Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 79.5 microns | 3.13 mil | estimated wet film thickness |
Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC) |